Wipe away the dust, oil and rust from the mold and remove the dirt on the surface before loading the mold to the injection molding machine. Use...
1. Processing aspects: (1) Excessive processing pressure, too fast speed, more filling, too long injection molding and pressure holding time will...
01 Improper feed adjustment, lack of material or excessive material Inaccurate feeding metering or abnormal feeding control system operation,...
Plastics are disturbed by gas during the filling process, and silver stripes or tiny bubbles often appear on the surface of the product or bubbles...
First, consider the issue of mold release. Secondly, considering the wall thickness of aluminum alloy die-casting, the thickness gap filled is...
1. Too high temperature will reduce the viscosity of the oil: when the temperature of injection molding is too high, the viscosity of the oil will...
At present, there is a classification on the market that divides all injection molding machines into servo injection molding machines and ordinary...
The injection temperature of pbt is 250 degrees Celsius, the scientific name of pbt is polybutylene terephthalate, and the color of pbt is milky...